Mixed bag

Stainless steel
1. Razor blade steels have 0.6% C although being stainless steel. justify.
2. What is the difference between KLA and weld decay , both being intergranular
corrosion?
3. Which is more corrosion resistant between FSS and ASS w.r.t: a) Pitting corrosion b) SCC
c) HIC and WHY?
4. Why is the increase in Ni in austenitic stanless steel first shows a dip in the time of
failure and then increase in time of failure w.r.t SCC?*
5. Why is delta ferrite increase lead to improvement in SCC ?
6. How is SFE important in SCC?*
7. Why are austenitic fillers used mostly in stainless steel welding?What is the problem of
ferritic and martensitic?
8. What are the 2 problems faced in austenitic weld metals?How is it overcome?
9. Why is ASS and FSS not heat treatable while MSS is?