Sie sind auf Seite 1von 1

Cold mechanical straightening process for C 54-2 column 1.

Firstly a study was carried out on the pattern of distortion through line checks at interval of 1m throughout the beam. 2. Jacks were used to apply pressure at points along the bend with intervals to bring into alignment. 3. The adjacent of the beam is adequately brace at the jacking position in order to prevent overloading. 4. The process was repeated until the beam is straightened within specific tolerance. 5. During the process the movement was observed to insure over straightening does not take place on either side of the beam.

Das könnte Ihnen auch gefallen