1.

0 introduction of IS2062 E250 grade A,B&C :-

IS 2062 is India standard covers the requirements of steel including micro-alloyed steel plates, strips,
shapes and section. this steel can be supplied in killed or semi killed condition and steel may ingot cast
or continuous casting

This standard has formerly known as IS226,now IS2062 has replaced this specification this grade steel is
for structural purposes . This grade is also commonly known as IS2062 GR E250(Fe-410-W).

This steel is subdivided into three types, i.e. grade A,B and C .

1.1.1- CHEMICAL COMPOSITION OF IS2062 E250 GRADE A:-

C Mn P S Si Carbon
equilent
(CE).MAX
0.23 1.50 0.045 0.045 0.40 0.42
TABLE-I

1.1.2- CHEMICAL COMPOSITION OF IS2062 E250 GRADE B:-

C Mn P S Si Carbon
equilent
(CE).MAX
0.22 1.50 0.045 0.045 0.40 0.41
TABLE-2

1.1.3- CHEMICAL COMPOSITION OF IS2062 E250 GRADE B:-

C Mn P S Si Carbon
equilent
(CE).MAX
0.20 1.50 0.045 0.045 0.40 0.39
TABLE-3
*composition in weight %age.

1.1.4- Micro alloying elements likes Nb , V, Ti mat be present in combination.


The limits are given below,

Grade Nb, V, Ti(max)


IS2062 E250 Grade A 0.25%
IS2062 E250 Grade B 0.25%
IS2062 E250 Grade C 0.25%
Table-2
2.0 MECHANICAL PROPERTIES OF IS2062 E250 GRADE A,B,C:-

IS2062 YS UTS % EL(MIN) BEND TEST HARDNESS CHARPY V-


GRADE N/mm2 N/mm2 (t) (RB) NOTCH IMPACT
E250 ENERGY (MIN)

A 250 Min 410 Min 23 3t - -


B 250 Min 410 Min 23 2t - 27 J at Room
temp See Note
C 250 Min 410 Min 23 2t - 27 J at Room
temp See Note
t : Nominal thickness of test piece, * : Elongation 15 min N in 80 mm GL for t 3.0 mm

Note: For grade IS 2062 E250 B,IS 2062 E250 C,E410,E450 D,E450 E Impact Test shall be certified
for product thickness of 12 mm or more. The testing temperature will be room temperature unless
otherwise specified in the order.

3.0 ;- METALLURGY OF IS 2062 E250 grade A,B &C;-