Sie sind auf Seite 1von 16

Field Joint of Cement lined Pipe

Field Joint of Cement lined Pipe

Fire Water Line

Fire Water Line
Prepared By          V.Johnson Prabu
Stages
• Mixing of coating material
• Surface preparation
• Application
• Joint fit‐up
• Welding
• Testing

Prepared By          V.Johnson Prabu
Coating Material
SINMAST
• SINMAST joining compound is used for 
bonding cement lined piping components.
• Sinmast is a 2 component , solvent free 
product based on Epoxy Resins
• Component A – Resin (0.945kg)
• Component B – Hardener (Ethylamine , 
Isopropylideendifenol) (0.055kg )

Prepared By          V.Johnson Prabu
Coating material
• Component A

• Component B 

Prepared By          V.Johnson Prabu
Coating Material
Mixing
• Both component A & B mixed together
• To avoid wastage it can be divided into 10 
parts and use it as required.
• The pot life of mixed component is 25min @ 
20o C approx. ( Working Time )
• The hardening time is 8hrs @ 20o C approx.

Prepared By          V.Johnson Prabu
Coating Material
Mixing
• Component A 
Total weight  = 945 gm
1/10 part  = 94.5 gm

Prepared By          V.Johnson Prabu
Coating Material
Mixing
• Usually One full cap of the can is equal to 1/10 
part. ( Measure it before mixing and conform)

Prepared By          V.Johnson Prabu
Coating Material
Mixing

Prepared By          V.Johnson Prabu
Surface Preparation
• The mating steel surface shall be free from oil, 
rust, burs and other foreign material.

Prepared By          V.Johnson Prabu
Application 
• Apply the mixed coating material gentily on 
the sleeve side at an angle of 45o approx.
• Remove the excess material.
• The join the mating surface and apply slight 
pressure. ( usually after joining you can find 
3mm difference )

Prepared By          V.Johnson Prabu
Application 

Prepared By          V.Johnson Prabu
Joint Fit‐up

Prepared By          V.Johnson Prabu
Joint Fit‐up
• Only tack weld the joint at three locations
• Remember : Joint shall be weld after 12 hrs

Prepared By          V.Johnson Prabu
Welding
• Do not move the joint after fit up.
• Support the line adequately to restrict the 
movement.
• After 12 hrs (ie; hardening time of coating 
material ) the joint is ready for welding.

Prepared By          V.Johnson Prabu
Welding
• Now the joint is ready for Further Testing

Prepared By          V.Johnson Prabu
Thank you !

Prepared By          V.Johnson Prabu

Das könnte Ihnen auch gefallen