This report summarizes corrosion data for a 0.5 km long carbon steel flowline with a 0.175 m outer diameter. The flowline transports crude oil with 73% CO2 and no H2S from 48.9°C and 3.8 bara at the inlet to 28.0°C and 3.4 bara at the outlet. Analysis shows a maximum corrosion rate of 4.2 mm/year at the inlet that decreases to 1.81 mm/year maximum by the outlet. No pitting corrosion was observed. Inhibitor treatment is available but at 0% efficiency.
This report summarizes corrosion data for a 0.5 km long carbon steel flowline with a 0.175 m outer diameter. The flowline transports crude oil with 73% CO2 and no H2S from 48.9°C and 3.8 bara at the inlet to 28.0°C and 3.4 bara at the outlet. Analysis shows a maximum corrosion rate of 4.2 mm/year at the inlet that decreases to 1.81 mm/year maximum by the outlet. No pitting corrosion was observed. Inhibitor treatment is available but at 0% efficiency.
This report summarizes corrosion data for a 0.5 km long carbon steel flowline with a 0.175 m outer diameter. The flowline transports crude oil with 73% CO2 and no H2S from 48.9°C and 3.8 bara at the inlet to 28.0°C and 3.4 bara at the outlet. Analysis shows a maximum corrosion rate of 4.2 mm/year at the inlet that decreases to 1.81 mm/year maximum by the outlet. No pitting corrosion was observed. Inhibitor treatment is available but at 0% efficiency.