1        Scope:  
 
This  specification  covers  the  requirements  for  the  supply  of  ASTM  A516  Gr  60N.    
 
2   Application:  
 
Plates  will  be  used  for  the  construction  of  Potable  Water  Tanks.    The  tank  will  be  built  for  Bu  
Hasa  Camp  Accommodation.  This  plate  material  is  used  for  tank  shell,  bottom,  bottom  annular  
and  roof  &  other  miscellaneous  items.    

3   Codes  and  Specifications  


 
Material  shall  be  supplied  in  accordance  with  following:  -­  
API  650  12th  Edition  Addendum  2,  ASTM  A20  and  ASTM  A516  Gr.  60  specification.  
 
4.   Chemical  Requirements:  
 
All  Chemical  properties  of  the  plates  supplied  shall  comply  with  requirements  of  ASTM  A516  Gr  
60.  
All  steel  shall  be  made  by  the  Basic  Oxygen  or  Electric  Furnace  process.    Mill  certificate  shall  
indicate  the  steel  making  process.  Bessemer  or  Rimmed  &  capped  steels  are  not  acceptable.  
Mill  shall  confirm  the  process  on  Material  test  certificate.  
 
5.   Mechanical  Properties:  
 
All  Mechanical  properties  of  the  plates  supplied  shall  comply  with  requirements  of  ASTM  A516  
Gr  60.  
 
6.   Heat  Treatment  
 
The  steel  shall  be  normalised.  
   
7.   Impact  Testing  
 
  Not  Applicable.    
 
   
8.   Ultrasonic  Testing  
 
Not  Applicable.  

 
 
 
 
 
9.   Surface  Imperfection  
 
Plates   shall  be   free  of  any   injurious   defects,   which   could   interfere   with  proper   fabrication  and  
construction.  Pitting  of  any  size  is  not  allowed.    
 
10.   Plate  Surface  Condition:    
 
Reworking  or  welding  on  plates  from  mill  is  not  acceptable.  All  surfaces  shall  be  free  of  cracks,  
imprint   of   scales,   scratches,   pitting’s,   and   deteriorated   surface   caused   by   lifting   devices.   No  
painting/coating  of  any  kind  is  permitted  on  the  steel  plates.  
 
11.   Tolerances  as  per  ASTM  A20:  
 
Thickness  under  tolerance:  Tolerance  on  thickness,  length  and  width  positive  as  per  ASTM  
A20  with  no  negative  tolerances.  
 
Out  of  square  tolerance:  The  out  of  square  of  a  plate  shall  be  limited  so  that  it  shall  be  possible  
to  inscribe  a  rectangle  with  the  dimensions  of  the  ordered  plate  within  the  delivered  size.  
 
12.   Documentation:  
 
The  material  shall  be  supplied  with  a  Material  Test  Certificate  type  3.1  in  accordance  with  EN-­
10204.  

13.   Marking  of  Plates  by  Mill:  


 
(i)   As   per   ASTM   A20,   and   in   addition   A6   Low   stress,   punching   &   painting   (stenciling),  
marking  required  on  two  locations  300mm  from  edges,  and  Mill  trade  name  /  monogram  
required  on  plate.  PO  No  &  VTC  name  inside  a  triangle  shall  be  marked.    
 
(ii)    As  per  ASTM  A20,  One  hard  stamp  of  Heat  Number  &  Plate  Number  and  One  Stencil  
marking.  
 