Type A
Random flake graphite
in a uniform distribution
Form I II III
Type B
Rosette flake graphite
Form IV V VI
largest flakes 1 (100 mm or more) 2 (50 -100 mm) 3 (25- 50 mm) 4 (12- 25 mm)
Type D
Undercooled
flake graphite
largest flakes 5 (6-12 mm) 6 (3-6 mm) 7 (1.5-3 mm) 8 (less than 1.5 mm)
Exploded graphite
Caused by high purity charge materials and
excess rare earth additions in high carbon
equivalent irons or in thicker section castings
largest nodules 6 (3-6 mm) 7 (1.5- 3 mm) 8 (less than 1.5 mm)
Inoculants
Elkem manufactures and markets a series of high quality inoculants to treat cast iron and ensure the production of the ideal graphite form, distribution and
freedom from chill (cementite). The following are examples taken from Elkem's extensive product portfolio.
Chunky graphite
Caused by high purity charge materials and
Inoculant Active Elements Advantages and Uses
excess rare earth additions in large section
Superseed® 75/50 Si Sr Low Al content. Low eutectic cell count through lower addition rates. High chill reduction.
castings or at high carbon equivalent
Ultraseed® Si Ca Ce (Al S O) High nodule count. Improved nodularity. Helps to prevent micro-shrinkage. Reactivates "dead" irons.
Superseed® Extra Si Sr Zr In addition to the advantages of Superseed® 75 inoculant, Superseed® Extra produces grey irons
with a refined graphite structure and enhanced mechanical properties.
All inoculants are available in sizes suitable for ladle or in-stream additions. Other inoculants for specialist applications are available.
Preconditioner
Product Active Elements Advantages and Uses
Spiky graphite
Preseed™ Si Al Ca Zr Preseed™ is a powerful preconditioning agent for all cast irons to improve consistency in melting
and increase mechanical properties. Caused by small amounts of tramp elements,
e.g. lead, bismuth, antimony and titanium,
Nodularisers in the absence of cerium
Elkem manufactures and markets a range of high quality nodularising alloys to produce ductile and compacted graphite cast irons. They contain balanced
ratios of the active elements to control reactivity, minimise slag and neutralise tramp elements.
Elkem AS, Foundry Products Division, Hoffsveien 65 b, P.O. Box 5211 Majorstua, N-0303 Oslo, Norway, www.foundry.elkem.com