CERTIFICATE OF CONFORMANCE Cleveland, Ohio 44117-1199 (APPLIES ONLY TO U.S. PRODUCTS)
Product: Shield-Arc® 85 [3Year]
Classification: E7010-A1 Specification: AWS A5.5:2006, ASME SFA-5.5 Date June 19, 2012 This is to certify that the product named above and supplied on the referenced order number is of the same classification, manufacturing process, and material requirements as the material which was used for the test that was concluded on the date shown, the results of which are shown below. All tests required by the specifications shown for classification were performed at that time and the material tested met all requirements. It was manufactured and supplied according to the Quality System Program of the Lincoln Electric Company, Cleveland, Ohio, U.S.A., which meets the requirements of ISO9001, NCA3800, AWS A5.01, and other specification and Military requirements, as applicable. The Quality System Program has been approved by ASME, ABS, and VdTUV. E7010-A1 Operating Settings Requirements RESULTS Electrode Size 313 1/8 1inch 5/322inch Polarity DC+ DC+ Plate Thickness, mm (in) 13 (1/2) 19 (3/4) Current, A 125 145 Pass/Layers 14/7 14/7 Preheat Temperature, °C (°F) (200 - 225) 95 (200) 95 (200) Interpass Temperature, °C (°F) (200 - 225) 105 (225) 105 (225) Postweld Heat Treatment 1 hour @ 1150°F 1 hour @ 620°C (1150°F) 1 hour @ 620°C (1150°F) Mechanical properties of weld deposits Tensile Strength, MPa (ksi) (70 min.) 620 (90) 560 (81) Yield Strength, 0.2% Offset, MPa (ksi) (57 min.) 520 (75) 460 (67) Elongation 22 min. 28 22 Average Hardness, HRB Not Required 93 88
Chemical composition of weld deposits (weight %)
C 0.12 max. 0.12 0.11 Mn 0.60 max. 0.58 0.40 Si 0.40 max. 0.23 0.12 S 0.03 max. 0.01 0.01 P 0.03 max. 0.01 0.01 Mo 0.40 - 0.65 0.54 0.57
1. This certificate complies with the requirements of EN 10204, Type 2.2.
2. The electrode sizes required to be tested for this classification are 1/8 inch and 5/32 inch. The 3/32 inch size will also meet these requirements. 3. Test assembly constructed of ASTM A204 Grade A steel. 4. Fillet Weld Test (positions as required): Met requirements. 5. Radiographic Inspection: Grade 2 - Met requirements. 6. Results below the detection limits of the instrument or lower than the precision required by the specification are reported as zero. Strength values in SI units are reported to the nearest 10 MPa converted from actual data. Preheat and interpass temperature values in SI units are reported to the nearest 5 degrees.
June 19, 2012 June 19, 2012
Toronto Cunningham, Certification Supervisor Date Dave Fink, Manager, Compliance Date Engineering, Consumable R&D