5.5 Surface Defects

Defect Name : Edge Burst (HR Defect)


Definition : These are serrated edges of hot rolled coil.

Defect Name : Coil Break Mark (HR Defect)


Definition : It is width-wise break lines commonly observed in Low Strength material at time of
processing.

Page 17 of 34 Steel Quality Guide V.1


SKM Steels Ltd
Defect Name : Rubbing Mark (HR Defect)
Definition : Rubbing mark or coil slip mark is a defect generated due to the rubbing action between the
consecutive wraps of coil. It appears bright and is easily visible.

Length

Defect Name : Lamination (HR Defect)


Definition : Lamination or peel off is caused due to non-metallic inclusion getting entrapped on slab
surface which gets dislodged during rolling.

Page 18 of 34 Steel Quality Guide V.1


SKM Steels Ltd
Defect Name : Sliver (HR Defect)
Definition : Sliver is caused due to slab surface defects like non-metallic inclusions, mould powder
entrapments getting open in subsequent hot or cold rolling.

Defect Name : Gouge Mark (HR Defect)


Definition : Observed in rolling direction. Some marks has depth and few appears only as surface
pattern, typically long.

Page 19 of 34 Steel Quality Guide V.1


SKM Steels Ltd
Defect Name : Fold Mark (HR Defect)
Definition : Fold mark generates by folding of strip which take place due to improper tension on strip
during rolling.

Defect Name : Black Boat Scale (HR Defect)


Definition : Black boat scale is un-removed primary and secondary scale which gets rolled on coil
surface along the rolling direction.

Page 20 of 34 Steel Quality Guide V.1


SKM Steels Ltd
Defect Name : Salt and Pepper Scale (HR Defect)
Definition : Salt and pepper scale is an attribute of worn out work roll of rolling stand.

Defect Name : High Temperature Scale (HR Defect)


Definition : Typically observed in V, W or M pattern on sheet surface. Impressions of worn out work roll
of stands gets embedded for formation of these type of defect.

Width

Page 21 of 34 Steel Quality Guide V.1


SKM Steels Ltd
Defect Name : Banded Scale (HR Defect)
Definition : It is a type of Rolled-in-Scale visible in V pattern.

Defect Name : Lump Mark (HR Defect)


Definition : Roll chip-off gives rise to lump mark on hot rolled coil surface. It is observed in pitch as per
diameter of roll.

Page 22 of 34 Steel Quality Guide V.1


SKM Steels Ltd
Defect Name : Lamination (CRCA Defect)
Definition : Lamination or peel off is caused due to non-metallic inclusion getting entrapped on slab
surface which gets dislodged during rolling.

Defect Name : MN Patch (CRCA Defect)


Definition : This type of patch has only boundaries and appears in yellow or brown color. It starts from
one edge of sheet due to eye vertical coil position.

Width

Page 23 of 34 Steel Quality Guide V.1


SKM Steels Ltd
Defect Name : Coolant Mark (CRCA Defect)
Definition : These are coolant drops rolled on cold rolled sheet surface.

Length

Defect Name : Emulsion Patch (CRCA Defect)


Definition : These are cracked emulsion residues on sheet surface. Observed in random distribution
over sheet surface and forms irregular shaped areas of dark discoloration.

Page 24 of 34 Steel Quality Guide V.1


SKM Steels Ltd
Defect Name : CC Patch (CRCA Defect)
Definition : Patches with dark brown to black in appearance. Here, with the map there is a blackish
substance within map. These are post annealing patch.

Defect Name : Sticker (CRCA Defect)


Definition : These are strained curved lines occurs as a result of inter lap sticking after batch
annealing. Mostly occur at middle of coil during unwinding.

Length

Page 25 of 34 Steel Quality Guide V.1


SKM Steels Ltd
Defect Name : Scum (CRCA Defect)
Definition : Defect appears in slightly inclined to rolling direction and scattered along the width. Gives
softer feeling to nails as it is a polyurethane material of damaged roll.

Defect Name : Alkali Patch (CRCA Defect)


Definition : It is a white color patch observed at strip edge. This patch is generated at ECL due to
improper rinsing and squeezing process.

Page 26 of 34 Steel Quality Guide V.1


SKM Steels Ltd

Defect Name : Zinc Run (Galvanised Defect)


Definition : Zinc run is the defect caused by improper wiping of excessive zinc after coil surface
passed through zinc bath

Defect Name : Sag Lines (Galvanised Defect)


Definition : Sag lines are the appearance defect of coated surface. Heavy coatings produced using a
slow line speed may suffer from a line defect referred to as sag-lines.

Page 27 of 34 Steel Quality Guide V.1


SKM Steels Ltd

Defect Name : Nozzle Streak (Galvanised Defect)


Definition : This is the defects of galvanized in which Lines of Zinc over-coating appears as streaks.
Appearance of this defect is dull finish from rest surface.

Defect Name : Dross (Galvanised Defect)


Definition : Dross is a mass of solid impurities floating on a molten Zinc bath or dispersed in the metal.

Page 28 of 34 Steel Quality Guide V.1


SKM Steels Ltd

Defect Name : Pot Roll Mark (Galvanised Defect)


Definition : Pot roll mark is the defect originated from a dross formation. When this dross growth takes
place on pot rolls, this created pot roll marks.

Defect Name : Lamination (Galvanised Defect)


Definition : It is surface defect on galvanised steel surface which has elongated metal flap and some
entrapped material below it. Flap is oriented in rolling direction.

Page 29 of 34 Steel Quality Guide V.1


SKM Steels Ltd

Defect Name : Pin Prick (Galvanised Defect)


Definition : The cold-rolled feed can be contaminated by a substance that prevents surface to get wet
during the hot dip. The strip surface becomes oxidized prior to entering the molten zinc pot
prevents coating.

Defect Name : Edge over coating (Galvanised Defect)


Definition : It is a build-up of extra coating at both the edges.

Page 30 of 34 Steel Quality Guide V.1


SKM Steels Ltd

Defect Name : Uncoated (Galvanised Defect)


Definition : This is the defects of galvanized in which few surface areas don't undergo coating.
Appearance of this defect is as blackish spot.

Defect Name : Hole (Galvanised Defect)


Definition : High severity lamination, slivers or casting blowholes gets opened during further rolling to
form holes.