Web Thickening

0.4

0.2 c/L

0.65 0.275

0.4 1.1 1.5 4.4


7
web thickness variation along span

Web Thickening
Section At c/L brg. deff L/8 TS 2L/8 3L/8 4L/8
Dist. From c/L brg. m 0 1.21 1.75 2.6 3.5 5.25 7

bw m 0.65 0.623 0.488 0.275 0.275 0.275 0.275

Overall depth of composite girder = 1.42 m


deff = 1.21 */Assumed 0.85 times of overall depth)

MATERIAL USED :
Grade of Reinforcement = Fe 500
fyk = 500 Mpa
Modulus of Elasticity Es = 200000 Mpa

Cast insitu deck = M 35


fck = 35 Mpa
fcm = 45 MPa
Ecm = 32000 MPa

Precast Beam = M 35
fck = 35
fcm = 45 MPa
Ecm = 32000 MPa

ANALYSES ASSUMPTION
Enviromental parameters
Relative humidity = 45 %
Exposure condition = Moderate

TEMPERATURE
Coefficent of thermal expansion = 1.2E-05 / C