METAL COMPOSTIONS

SA-212 SA-285 SA-301 SA-210


Composition Composition Composition Composition
C 0.28-0.35 C 0.15-0.30 C 0.18-0.25 C 0.10-0.2
Cr \ Cr \ Cr 0.50-0.70 Cr \
Mn 0.9 Mn 0.8 Mn 0.8 Mn 0.8
S 0.05 S 0.05 S 0.05 S 0.045
P 0.035-0.04 P 0.035-0.05 P 0.035-0.04 P 0.04
Si 0.15-0.30 Si \ Si 0.15-0.3 Si \
Mo \ Mo \ Mo 0.40-0.60 Mo \
Ni \ Ni \ Ni \ Ni \

Properites Properites Properites Properites


Ultimate Strength psi 65,000-82,000 Ultimate Strength psi 45,000-32,500 Ultimate Strength psi 70,000-82,000 Ultimate Strength psi 59,750
Yield Stength psi 32,500-41,000 Yield Stength psi 22,500-32,500 Yield Stength psi 38,000-45,100 Yield Stength psi 42,450
Hardness Brinell Hardness Brinell Hardness Brinell Hardness Brinell 117
Melting point Melting point Melting point Melting point 950 F
Thermal conductivity Thermal conductivity Thermal conductivity Thermal conductivity

SA-209 GRT1a SA-213(SA335P2) SA-213 GRT11 SA-213 GR T3b


Composition Composition Composition Composition
C 0.1-0.2 C 0.1-0.2 C 0.15 C 0.15
Cr \ Cr 0.5-0.7 Cr 1.00-1.50 Cr 1.75-2.25
Mn 0.3-0.8 Mn 0.3-0.6 Mn 0.3-0.6 Mn 0.3-0.6
S 0.045 S 0.05 S 0.03 S 0.03
P 0.04 P 0.04 P 0.03 P 0.03
Si 0.1-0.5 Si 0.1-0.3 Si 0.5-1 Si 0.5
Mo 0.45-0.65 Mo 0.45-0.65 Mo 0.45-0.65 Mo 0.45-0.65
Ni Ni Ni Ni

Properites Properites Properites Properites


Ultimate Strength psi 63,000 Ultimate Strength psi 69,200 Ultimate Strength psi 74,200 Ultimate Strength psi 69,450
Yield Stength psi 49,000 Yield Stength psi 34,600 Yield Stength psi 55,100 Yield Stength psi 46,200
Hardness Brinell 141 Hardness Brinell 130 Hardness Brinell 153 Hardness Brinell 140
Melting point 975 F Melting point 975 F Melting point 1050 F Melting point 1080 F
Thermal conductivity Thermal conductivity Thermal conductivity Thermal conductivity
METAL COMPOSTIONS
SA-209 GRT1a SA-213(SA335P2) SA-213 GRT11 SA-213 GR T3b
Composition Composition Composition Composition
C 0.1-0.2 C 0.1-0.2 C 0.15 C 0.15
Cr \ Cr 0.5-0.7 Cr 1.00-1.50 Cr 1.75-2.25
Mn 0.3-0.8 Mn 0.3-0.6 Mn 0.3-0.6 Mn 0.3-0.6
S 0.045 S 0.05 S 0.03 S 0.03
P 0.04 P 0.04 P 0.03 P 0.03
Si 0.1-0.5 Si 0.1-0.3 Si 0.5-1 Si 0.5
Mo 0.45-0.65 Mo 0.45-0.65 Mo 0.45-0.65 Mo 0.45-0.65
Ni Ni Ni Ni

Properites Properites Properites Properites


Ultimate Strength psi 63,000 Ultimate Strength psi 69,200 Ultimate Strength psi 74,200 Ultimate Strength psi 69,450
Yield Stength psi 49,000 Yield Stength psi 34,600 Yield Stength psi 55,100 Yield Stength psi 46,200
Hardness Brinell 141 Hardness Brinell 130 Hardness Brinell 153 Hardness Brinell 140
Melting point 975 F Melting point 975 F Melting point 1050 F Melting point 1080 F
Thermal conductivity Thermal conductivity Thermal conductivity Thermal conductivity

SA-213 GR T22 SA-213 GR T21 SA-213 GR T5 SA-213 GR T9


Composition Composition Composition Composition
C 0.15 C 0.15 C 0.15 C 0.15
Cr 2.00-2.50 Cr 2.75-3.25 Cr 4.00-6.00 Cr 8.00-10.00
Mn 0.3-0.6 Mn 0.3-0.6 Mn 0.3-0.6 Mn 0.3-0.6
S 0.03 S 0.03 S 0.03 S 0.03
P 0.03 P 0.03 P 0.03 P 0.03
Si 0.5 Si 0.5 Si 0.5 Si 1
Mo 0.9-1.10 Mo 0.8-1 Mo 0.45-0.65 Mo 0.45-0.65
Ni Ni Ni Ni

Properites Properites Properites Properites


Ultimate Strength psi 69,900 Ultimate Strength psi 69,100 Ultimate Strength psi 69,800 Ultimate Strength psi 73,460
Yield Stength psi 45,080 Yield Stength psi 40,100 Yield Stength psi 38,600 Yield Stength psi 43,470
Hardness Brinell 147 Hardness Brinell 146 Hardness Brinell 139 Hardness Brinell 145
Melting point 1100 F Melting point 1125 F Melting point 1150 F Melting point 1200 F
Thermal conductivity Thermal conductivity Thermal conductivity Thermal conductivity
METAL COMPOSTIONS
SA-213 GR T22 SA-213 GR T21 SA-213 GR T5
Composition Composition Composition
C 0.15 C 0.15 C 0.15
Cr 2.00-2.50 Cr 2.75-3.25 Cr 4.00-6.00
Mn 0.3-0.6 Mn 0.3-0.6 Mn 0.3-0.6
S 0.03 S 0.03 S 0.03
P 0.03 P 0.03 P 0.03
Si 0.5 Si 0.5 Si 0.5
Mo 0.9-1.10 Mo 0.8-1 Mo 0.45-0.65
Ni Ni Ni

Properites Properites Properites


Ultimate Strength psi 69,900 Ultimate Strength psi 69,100 Ultimate Strength psi 69,800
Yield Stength psi 45,080 Yield Stength psi 40,100 Yield Stength psi 38,600
Hardness Brinell 147 Hardness Brinell 146 Hardness Brinell 139
Melting point 1100 F Melting point 1125 F Melting point 1150 F
Thermal conductivity Thermal conductivity Thermal conductivity

SA-376 TYPE 347 SA-376 TYPE 347 SA-213 GR T9


Composition Composition Composition
C 0.8 C 0.8 C 0.15
Cr 16-18 Cr 16-18 Cr 8.00-10.00
Mn 2 Mn 2 Mn 0.3-0.6
S 0.03 S 0.03 S 0.03
P 0.03 P 0.03 P 0.03
Si 0.75 Si 0.75 Si 1
Mo 2.00-3.00 Mo 2.00-3.00 Mo 0.45-0.65
Ni Ni Ni

Properites Properites Properites


Ultimate Strength psi 84,000- Ultimate Strength psi 84,000- Ultimate Strength psi 73,460
Yield Stength psi 43,660 Yield Stength psi 43,660 Yield Stength psi 43,470
Hardness Brinell Hardness Brinell Hardness Brinell 145
Melting point Melting point Melting point 1200 F
Thermal conductivity Thermal conductivity Thermal conductivity