THE REASON I DEVELOPED THIS SYSTEM WAS FOR FIRST-TIMERS THAT WANTED
TO TRY WORKING WITH GOLD BUT DID NOT WANT ANY TOXIC ACIDS.EVEN
MORE IMPORTANTLY YOU CANNOT LOSE ANY GOLD BY MAKING A MISTAKE!
LET THE MIXTURE SIT FOR 24 HOURS, STIRRING THE MIXTURE EVERY 8 HOURS.
(THE SODIUM NITRATE WILL NOT DESOLVE COMPLETELY)
YOU NOW HAVE A HOMEMADE NITRIC ACID THAT IS APPROX 70% AS STRONG AS
FULL STRENGTH NITRIC.
STIR THE MIX DAILY AND JUST ADD MORE SULFURIC ACID AFTER YOU POUR
OFF THE MIXED ACID.
Survival Page 1
PLACE THE MATERIAL IN A CLEAR GLASS OR PLASTIC CONTAINER (HDPE
PLASTIC).
ADD THE NITRIC SUBSTITUTE ACID ,JUST ENOUGH TO COVER THE MATERIALS.
WITHOUT HEATING THE BATH IT WILL TAKE 3 TO 10 DAYS FOR THE ACID TO
DESOLVE ALL THE NON-GOLD METALS.
IF YOU HEAT THE BATH IT CAN BE FINISHED IN HOURS INSTEAD OF DAYS.
POUR OFF THE BATH THROUGH A PAINT FILTER TO CATCH THE GOLD FLAKES
AND PINS THAT ARE FLOATING.
IF YOUR BATH HAS REAL FINE GOLD DUST THAT ESCAPES THROUGH THE PAINT
FILTERS THEN REFILTER THE LIQUIDS WITH A COFFEE FILTER TO CATCH THE
GOLD DUST
(THE WASTE ACID MIGHT CONTAIN SILVER, JUST ADD UN-IODIZED SALT TO THE
ACID,IF SILVER IS PRESENT IT WILL DROP TO THE BOTTOM AS A WHITE
MUD/CURD)
THEN NEUTRALIZE THE WASTE ACID WITH UREA , THEN WITH BAKING SODA.
NOW REFILL YOUR BATH CONTAINER WITH WATER TO RINSE THE REST OF THE
GOLD OFF THE MATERIALS.
USING A PAIR OF STAINLESS STEEL TWEEZERS YOU CAN PICKUP THE
MATERIALS AND RINSE THE GOLD OFF WITH WATER.
REPEAT THE POUR-OFF THROUGH A PAINT FILTER TO CATCH THE GOLD.
NOW USING JUST WATER TAKE ALL THE PAINT FILTERS AND RINSE THE GOLD
OUT OF THE FILTERS INTO A CLEAN CONTANER.
LET IT SET UNTIL THE GOLD SETTLES TO THE BOTTOM, SLOWLY POUR OFF THE
WATER.
IF YOUR BATH HAS REAL FINE GOLD DUST THAT ESCAPES THROUGH THE PAINT
FILTERS THEN REFILTER THE LIQUIDS WITH A COFFEE FILTER TO CATCH THE
GOLD DUST.